Nanjing Suntech Metal Equipment Co., Ltd.

PROFESSIONAL DESIGN SUPERIOR MANUFACTURING EXCELLENT PRODUCTS QUALITY SERVICE

Manufacturer from China
Active Member
10 Years
Home / Products / Titanium Clad Plate /

Gr.12 / 516 Gr.70N Titanium Clad Plate Tubesheet for Anti-pitting Corrosion

Contact Now
Nanjing Suntech Metal Equipment Co., Ltd.
City:nanjing
Province/State:jiangsu
Country/Region:china
Contact Person:MsMargaret Xiao
Contact Now

Gr.12 / 516 Gr.70N Titanium Clad Plate Tubesheet for Anti-pitting Corrosion

Ask Latest Price
Brand Name :Suntech
Model Number :E0018
Certification :EN10204 3.1, EN10204 3.2, DNV, TUV, SGS, etc
Place of Origin :P.R.China
MOQ :1 piece
Price :negotiation
Payment Terms :L/C, D/A, T/T, D/P,etc
Supply Ability :35000tons/Year
Delivery Time :60 working days after received your payment
Packaging Details :Seaworthy packing
Cladding Material :SB265 Gr.12
Base Material :SA516 Gr.70N
Size :(10+70)*OD1700mm
Max. Size :28sqm
Production Code :ASTM B898, ASME SB898
Surface Treatment :Auto Polished
more
Contact Now

Add to Cart

View Product Description

Gr.12 / 516 Gr.70N Titanium Clad Plate Tubesheet for Anti-pitting Corrosion

Description:

Clad plates provide an economical solution for chemical processing. Explosion welding is a solid state joining process in which explosive energy is used to propel the component metal parts together to form a metallurgical bond. At the point of impact of the two components, a thin layer is stripped from both colliding surfaces and is ejected as a molten metal jet. This jet contains the surface contaminants and oxides that would otherwise prevent bonding. The two surfaces are in intimate contact under extreme pressure enabling the bond to be formed.

Table for available type of titanium clad plates:

Product Names:

Titanium Clad Plate/Sheet, Titanium Clad Tube Sheet/ Tube Plate

Production Codes:

ASTM B898, ASME SB898, ASTM B264, ASME SB264, ASTM B265, ASME SB265, ASTM B432, ASME SB432, DIN , BS, JIS, GB/T, ISO, etc.

Titanium Grades:

ASTM/ASME B265 Gr1, Gr2, Gr.3, Gr.5, Gr7, Gr.9, Gr12

Form

Description

Base Layer

Base Layer Grade

Maximum Size

Clad Plate

Titanium / Carbon Steel Clad

Carbon steel plate and forging

SA516 Gr.60(N),Gr.70(N),SA387 Gr.11, Gr.22, SA266, SA350, etc.

(1.5~14)/(2~200) x W(max W 4110) x L(max L 7000)

Titanium / Stainless Steel (Duplex) Clad

Duplex, Stainless Steel & their forgings

304L,316L, 316Ti, 321, 317L, 310S, 410S, 904L, 1805, 2205, 2507, Al6XN, 254sMo,etc.

(1.5~14)/(2~200) x W(max W 4110) x L(max L 7000)

Titanium / Copper (Naval Brass) Clad

Copper, Naval Brass

C10100, C10200, C11000, C26200, C28000, C46400, C70600, C71500, etc.

(1.5~14)/(2~100) x W(max W 2100) x L(max L 6000)

Titanium / Aluminum Clad

Aluminum

A1050, A1060, A1070, A1100, A5052, etc.

(1.5~14)/(6~50) x W(max W 1500) x L (max L 4000)

Titanium / Nickel Clad

Nickel and its alloy

N02200, Monel 400, Inconel 600, Incoloy 800, 825, C276, C22, etc

(1.5~14)/(6~50) x W(max W 2000) x L (max L 5000)

Titanium / Carbon Steel / Titanium Clad

Carbon steel plate and forging

SA516 Gr.60(N),Gr.70(N),SA387 Gr.11, Gr.22, SA266, SA350, etc.

(1.5~14)/(6~200)/(1~10) x W(max W 3000) x L(max L 6000)

Titanium / Copper / Titanium Clad

Copper, Naval Brass

C10100, C10200, C11000, C26200, C28000, C46400, C70600, C71500, etc.

(1.5~14)/(2~100) x W(max W 2100) x L(max L 6000)

Titanium / Carbon Steel / Stainless Steel Clad

Carbon steel plate and forging

SA516 Gr.60(N),Gr.70(N),SA387 Gr.11, Gr.22, SA266, SA350, etc.

(1.5~14)/(6~200)/(1.5~10) x W(max W 4110) x L(max L 7000)

Duplex, Stainless Steel & their forgings

304L,316L, 316Ti, 321, 317L, 310S, 410S, 904L, 1805, 2205, 2507, Al6XN, 254sMo,etc.

Zirconium / Titanium / Carbon Steel Clad

Zirconium

R60702

(1.5~14)/(1.5~2)/(2~200) x W(max W 4110) x L(max L 7000)

Carbon steel plate and forging

SA516 Gr.60(N),Gr.70(N),SA387 Gr.11, Gr.22, SA266, SA350, etc.

Aluminum / Titanium / Carbon Steel Clad

Aluminum

A1050, A1060, A1070, A1100, A5052, etc.

(1.5~40)/(1-5)/(8~200) x W(max W 1000) x L(max L 1000)

Carbon steel plate and forging

SA516 Gr.60(N),Gr.70(N),SA387 Gr.11, Gr.22, SA266, SA350, etc.

Aluminum / Titanium / Copper Clad

Aluminum

A1050, A1060, A1070, A1100, A5052, etc.

(1.5~40)/(1-5)/(1~100) x W(max W 1000) x L(max L 1000)

Copper, Naval Brass

C10100, C10200, C11000, C26200, C28000, C46400, C70600, C71500, etc.

Application: Petro-chemical, Vacuum Salt Industry, Chlor-alkali, Metallurgical, Food, Light Industry, Medicine, Auto Industry, Electrolytic Aluminum, Fertilizer, Kitchenware, Power Industry, Building Materials,Electrolysis Industry, Hydrometallurgy etc.

Competitive Advantage:

Competitive Advantage

1. Abundant experience

- More than one decade of abundant experience in non-ferrous metal cladding and production;

- Miscellaneous metals cover Nickel Alloy, Titanium Alloy, Copper-Nickel Alloy, Zirconium, Tantalum Alloy, Super Stainless Steel;

- Produced according to ASTM, ASME, JIS, DIN, ISO other codes;

- Over 20 items of inventory or practical new-type patents.

2. Professional technical consulting service

- Generate technical specification to adopt in local market;

- Technical bid evaluation and clarification;

- Supplier technical document review, such as inspection and test plan, WPS / PQR, fabrication procedures, etc.;

- Technical consulting on material, welding, NDE, etc.;

- Non-conformance solution consulting;

- Others that might be requested by customer.

3. Independent inspection service

- Technical clarification with customer;

- Attend / organize pre-inspection meeting;

- In-process inspection, including: Material inspection, Test witness, Visual & dimensional inspection, Welding inspection, NDE inspection, Coating inspection;

- Final inspection on finished products;

- Packing inspection;

- Progress report and schedule expediting;

- Other inspection might be requested by customer.

4. Transportation advantage

- 296kms away from Shanghai seaport

Production Procedure:

Gr.12 / 516 Gr.70N Titanium Clad Plate Tubesheet for Anti-pitting Corrosion

Gr.12 / 516 Gr.70N Titanium Clad Plate Tubesheet for Anti-pitting Corrosion

Inquiry Cart 0
You May Like
SB265 Gr.7 Titanium Clad Plate Tubesheet for Anti-crevice Corrosion
SB265 Gr.7 Titanium Clad Plate Tubesheet for Anti-crevice Corrosion
Explosin Bonded Clad Plate B265 Gr2 / A516 Gr 70 Titanium / Steel Clad Square Plate
Explosin Bonded Clad Plate B265 Gr2 / A516 Gr 70 Titanium / Steel Clad Square Plate
Cladding Plate  SB265 Gr.1 Titanium / Carbon Steel Clad Tubesheet
Cladding Plate SB265 Gr.1 Titanium / Carbon Steel Clad Tubesheet
Explosin Bonded SB265 Gr.1 / Q235B Titanium Clad Strip for Electrolyation
Explosin Bonded SB265 Gr.1 / Q235B Titanium Clad Strip for Electrolyation
SB265 Gr.1 / 516 Gr.70N Titanium Clad Plate for Heat Exchanger Tubesheets
SB265 Gr.1 / 516 Gr.70N Titanium Clad Plate for Heat Exchanger Tubesheets
Gr.2 / 516 Gr.70N Titanium Clad Plate Square Tubesheet for Steam Turbine
Gr.2 / 516 Gr.70N Titanium Clad Plate Square Tubesheet for Steam Turbine
Gr.12 / 516 Gr.70N Titanium Clad Plate Tubesheet for Anti-pitting Corrosion
Gr.12 / 516 Gr.70N Titanium Clad Plate Tubesheet for Anti-pitting Corrosion
Drilled B265 Gr2 / SA105 Explosion Bonded Clad Plate Tubesheet for Heat Exchangers
Drilled B265 Gr2 / SA105 Explosion Bonded Clad Plate Tubesheet for Heat Exchangers
SB265 Gr.1 Titanium Clad Plate Square Tubesheet Auto Polished Inner Surface Treatment
SB265 Gr.1 Titanium Clad Plate Square Tubesheet Auto Polished Inner Surface Treatment
Explosin Bonded SB265 Gr.1 / A516 Gr.70N Titanium Clad Steel Plates for Evaporators
Explosin Bonded SB265 Gr.1 / A516 Gr.70N Titanium Clad Steel Plates for Evaporators
SB265 Gr.1 Titanium / Carbon Steel Clad Tubesheet for Condensers
SB265 Gr.1 Titanium / Carbon Steel Clad Tubesheet for Condensers
SB265 Gr.2 Titanium Clad Plate for Flue Gas Desulfurization FGD
SB265 Gr.2 Titanium Clad Plate for Flue Gas Desulfurization FGD
SB265 Gr.1 Titanium Clad Plate
SB265 Gr.1 Titanium Clad Plate
B265 Gr2 / SA105 Titanium Clad Plate
B265 Gr2 / SA105 Titanium Clad Plate
Explosin Bonded Clad Plate / Tubesheet
Explosin Bonded Clad Plate / Tubesheet
Send your message to this supplier
*From:
*To:

Nanjing Suntech Metal Equipment Co., Ltd.

*Subject:
*Message:
Characters Remaining : (0/3000)
Contact Now